Plasticization of an ionic thermoplastic elastomer based on a zinc sulfonated ethylene—propylene—diene terpolymer of high ethylene content
作者: Thomas KurianD. KhastgirP.P. DeD.K. TripathyS.K. De
作者单位: 1Rubber Technology Centre, Indian Institute of Technology, Kharagpur 721 302, India
刊名: Polymer, 1996, Vol.37 (3), pp.413-419
来源数据库: Elsevier Journal
DOI: 10.1016/0032-3861(96)82910-7
关键词: zinc sulfonated EPDMplasticizationthermoplastic elastomer
原始语种摘要: Abstract(#br)Zinc sulfonated ethylene—propylene—diene terpolymer (EPDM) behaves as an ionic thermoplastic elastomer. Both paraffin oil and dimethyl sulfoxide (DMSO) act as plasticizers for this polymer; while paraffin oil plasticizes the hydrocarbon backbone, DMSO plasticizes the ionic domains. Results obtained from dynamic mechanical analysis (d.m.a.) show that DMSO does not affect the glass—rubber transition temperature ( T g ), occurring at around −26°C, but adversely affects the broad transition in the temperature range from +27 to +80°C, which is believed to be due to the hard phase resulting from the ionic aggregates in the polymer. Paraffin oil, however, causes a lowering of the T g (from −26 to −34°C) without affecting the high-temperature transition. Results obtained from...
全文获取路径: Elsevier  (合作)
分享到:
来源刊物:
影响因子:3.379 (2012)

×
关键词翻译
关键词翻译
  • elastomer 弹性体
  • sulfonated 磺化
  • thermoplastic 热塑性塑料
  • terpolymer 三元共聚物
  • propylene 丙烯
  • diene 二烯
  • ionic 离子的
  • transition 转移
  • plasticization 塑性化
  • ethylene 乙烯